Causes and solutions of top whiteness in injection molding products

Release time:2021-08-16

When the plastic parts of injection products are ejected from the mold, if the ejector pin is used, the ejector rod will often leave deep or shallow marks on the plastic parts. If these traces are too deep, the so-called top white phenomenon will appear. In serious cases, the so-called top explosion will occur when the plastic parts are pushed through.


The main reason for the whiteness of plastic parts is that the product has a large mold adhesion force, and the ejection part on the plastic parts causes white marks at the ejection part of the ejector rod. The specific reasons and improvement methods are as follows:


1. Back mold temperature is too low or too high: adjust the appropriate mold temperature.


2. Too fast ejection speed: slow down the ejection speed.


3. With demoulding chamfer: overhaul the mold (polishing).


4. The ejection of finished products is unbalanced (the ejection leaf spring is broken): repair the mold (make the ejection balanced).


5. Insufficient number of thimbles or improper position: increase the number of thimbles or change the position of thimbles.


6. Vacuum occurs in the mold during demoulding: clean the dirt in the ejector pin hole to improve the air inlet effect.


7. The finished bone and column positions are rough (inverted): polish each bone and column position.


8. High injection pressure or holding pressure: reduce the pressure appropriately.


9. The demoulding angle of the finished mold is too small: increase the demoulding angle of the rear mold.


10. Improper action time or position of side slider: repair the mold (make the core pulling action normal).


11. Ejection area is too small or ejection speed is too fast: increase the ejection area or slow down the ejection speed.


12. The injection speed of the last section is too fast (Burr): slow down the injection speed of the next section.


These are the reasons and solutions for the whitening of injection molded products.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
主站蜘蛛池模板: 三级在线免费观看 | 婷婷性 | 日日摸夜夜添夜夜添成人 | 中国女人特级毛片 | 日本亚州视频在线八a | 午夜视频免费 成人 | 色综合综合在线 | 日日干日日摸 | 在线视频自拍 | 啪啪免费网 | 污视频在线观看视频 | 色久月 | 啪啪免费小视频 | 天堂网在线资源www最新版 | 自拍亚洲 | 亚洲激情视频 | 亚洲三级网站 | 亚洲日本在线观看网址 | 四虎永久免费影院在线 | 亚洲资源最新版在线观看 | 日本不卡免费新一区二区三区 | 日本欧美高清全视频 | 日本三区四区免费高清不卡 | 一二三四在线观看高清在线观看一 | 亚洲资源最新版在线观看 | 四虎影视免费 | 日韩一级一片 | 五月婷婷综合网 | 最新版天堂中文在线官网 | 日韩欧美色视频在线观看 | 中文字幕亚洲无线码在一区 | 日本在线观看一区二区三区 | 午夜在线播放免费高清观看 | 欧美在线黄色 | 午夜激爽毛片在线看 | 色综合久久综精品 | 在线成人免费观看国产精品 | 欧美一级片网址 | 少妇激情av一区二区 | 亚洲综合色婷婷六月丁香 | 日韩欧美三级视频 |