Solution to lack of glue in plastic shell

Release time:2023-11-29

Lack of glue, also known as insufficient filling, is one of the common problems in the process of injection molding. The injection molding part is not full, and the existing bubbles, cavities, shrinkage holes, etc. are inconsistent with the standard template, which is called lack of glue. So how to solve itPlastic shellWhat about the lack of glue?

圖片2.png


The following are the reasons for the lack of glue in the plastic shell and its improvement measures:


① Mold: a. the design of the gating system is unreasonable. The gating system is the channel for the melt to enter the mold cavity, which has a great impact on the molding quality of the plastic parts. The gate is not parallel and the gate is not located at the wall thickness; b. The exhaust structure of the mold is poor; c. Impurities or cold materials in the melt block the flow channel; d. Mold temperature does not meet the requirements. Improvement measures: improve the pouring system, increase the exhaust of the mold, remove the impurities of the compound, and increase the mold temperature.


② Raw materials: a. the water content of raw materials is too large; b. Volatile substances in raw materials exceed the standard; c. There are too many impurities or recycled materials in the raw materials. Improvement measures: barbecue raw materials and increase raw materials.


③ Injection molding machine: A. insufficient injection quantity: for example, 180t products are produced by 150t machines. b. The nozzle is blocked by foreign matters and the nozzle hole is too small; c. Insufficient supply of raw materials: if the barrel is blocked, the nozzle material will affect the blanking; d. Check valve failure; e. Insufficient injection stroke. Improvement measures: increase the injection volume and increase the injection stroke.


④ Molding operation: A. mold temperature is too low; b. The injection pressure is too low; c. The pressure holding time is too short; d. The injection speed is too slow; e. The melt temperature is too low. Improvement measures: increase the mold temperature, increase the injection pressure, maintain the pressure time, and improve the injection speed.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
主站蜘蛛池模板: 日本理论在线 | 在线观看男女爱视频网站 | 亚洲欧美日韩成人网 | 人与禽交免费网站视频 | 日韩免费视频 | 三级黄色片日韩 | 欧美视频中文字幕 | 亚洲激情欧美 | 亚洲黄色网址大全 | 青青草好 | 四虎最新永久在线精品免费 | 青青草一区 | 天天色天天射天天干 | 欧美视频免费 | 一二三四视频社区在线网 | 中文字幕欧美在线观看 | 色天网站 | 午夜传媒| 天天插狠狠干 | 青青操原 | 青草园网站在线观看 | 欧美一级成人一区二区三区 | 一级毛片视频免费 | 日本卡一卡2卡3卡4精品卡网站 | 亚洲最新中文字幕 | 日本天堂视频 | 青青草免费公开视频 | 四虎成人免费影院网址 | 天堂网在线资源 | 日韩精品视频免费网址 | 伊人影视大全 | 欧美一级特黄aaaaaa在线看片 | 青草99| 欧美在线xx| 欧美性猛交一区二区三区 | 欧美亚洲综合一区 | 日本精品一区 | 五月婷婷六月丁香在线 | 色天使在线播放 | 色噜噜狠狠色综合中文字幕 | 小明永久成人一区二区 |